Al2O3 Atomic Layer Deposition on Nanostructured ..gamma..-Mg(BH4)2 for H2 Storage

Noemie Marius, Nicholas Strange, Andreas Schneemann, Vitalie Stavila, Karl Gross, Nancy Washton, Madison Martinez, Thomas Gennett, Steven Christensen

Research output: Contribution to journalArticlepeer-review

19 Scopus Citations

Fingerprint

Dive into the research topics of 'Al2O3 Atomic Layer Deposition on Nanostructured ..gamma..-Mg(BH4)2 for H2 Storage'. Together they form a unique fingerprint.

Material Science