TY - GEN
T1 - Atomic Layer Deposition for Improved Biomass Conversion Catalysts
AU - McNeary, W.
PY - 2021
Y1 - 2021
N2 - Heterogeneous catalysts are a key enabler of the transition towards a sustainable, bio-based economy for fuels and chemicals. However, the harsh conditions in many biomass conversion processes lead to nanoparticle sintering, support collapse, and metal leaching in conventional PGM catalysts. Next-generation catalysts must be developed to address these stability challenges. This presentation will discuss ongoing work between the Catalytic Carbon Transformation and Scale-Up Center at NREL and various industrial partners to develop scalable and cost-effective atomic layer deposition (ALD) coatings for improving the performance of biomass conversion catalysts. The substantial focus will be devoted to the benefits of TiO2 ALD coatings on supported Pd hydrogenation catalysts. Ten cycles of TiO2 ALD were found to dramatically improve the activity of a conventional Pd/Al2O3 catalyst towards aromatic hydrogenation, despite partial coverage of the Pd sites by the ALD layer. Subsequent advanced characterization and atomic-scale computational modeling revealed that the ALD coating weakened the adsorption strength of hydrogenation surface intermediates, leading to higher reaction rates. Reaction testing after exposure to sulfur impurities, high temperature oxidation, and hydrothermal treatment demonstrated the improved stability of the ALD-coated catalyst. Additionally, the ALD synthesis process was found to be scalable over two orders of magnitude with minimal deviation in synthesized catalyst properties. These results were contextualized with cost models of industrial ALD coating and aromatic hydrogenation processes to further refine the value proposition of ALD coatings. Given the demonstrated improvements in hydrogenation, TiO2 ALD coatings have also been applied to supported Pt catalysts for use in other biomass conversion reactions, such as hydrodeoxygenation for the production of sustainable aviation fuel (SAF) and the oxidation of glucose to bio-derived gluconic acid.
AB - Heterogeneous catalysts are a key enabler of the transition towards a sustainable, bio-based economy for fuels and chemicals. However, the harsh conditions in many biomass conversion processes lead to nanoparticle sintering, support collapse, and metal leaching in conventional PGM catalysts. Next-generation catalysts must be developed to address these stability challenges. This presentation will discuss ongoing work between the Catalytic Carbon Transformation and Scale-Up Center at NREL and various industrial partners to develop scalable and cost-effective atomic layer deposition (ALD) coatings for improving the performance of biomass conversion catalysts. The substantial focus will be devoted to the benefits of TiO2 ALD coatings on supported Pd hydrogenation catalysts. Ten cycles of TiO2 ALD were found to dramatically improve the activity of a conventional Pd/Al2O3 catalyst towards aromatic hydrogenation, despite partial coverage of the Pd sites by the ALD layer. Subsequent advanced characterization and atomic-scale computational modeling revealed that the ALD coating weakened the adsorption strength of hydrogenation surface intermediates, leading to higher reaction rates. Reaction testing after exposure to sulfur impurities, high temperature oxidation, and hydrothermal treatment demonstrated the improved stability of the ALD-coated catalyst. Additionally, the ALD synthesis process was found to be scalable over two orders of magnitude with minimal deviation in synthesized catalyst properties. These results were contextualized with cost models of industrial ALD coating and aromatic hydrogenation processes to further refine the value proposition of ALD coatings. Given the demonstrated improvements in hydrogenation, TiO2 ALD coatings have also been applied to supported Pt catalysts for use in other biomass conversion reactions, such as hydrodeoxygenation for the production of sustainable aviation fuel (SAF) and the oxidation of glucose to bio-derived gluconic acid.
KW - atomic layer deposition
KW - catalysis
M3 - Presentation
T3 - Presented at the ALD/ALE 2021 Virtual Meeting, 28 June 2021
ER -