Interfacial Engineering by Atomic Layer Deposition for Highly Durable and Safe Lithium-Ion Batteries: Abstract 551

Ahmad Pesaran, Chunmei Ban, Yoon Seok Jung, Anne Dillion, Steven George, See Hee Lee, Gi-Heon Kim, Andrew Cavanagh

Research output: Contribution to conferencePaper

Original languageAmerican English
Number of pages1
StatePublished - 2010
Event218th Meeting of The Electrochemical Society (ECS) - Las Vegas, Nevada
Duration: 10 Oct 201015 Oct 2010

Conference

Conference218th Meeting of The Electrochemical Society (ECS)
CityLas Vegas, Nevada
Period10/10/1015/10/10

NREL Publication Number

  • NREL/AB-5400-51886

Keywords

  • ALD
  • anode
  • atomic layer deposition
  • cathode
  • Li-ion batteries

Cite this